Common Standard Alloy Wheel used in Germany

Heat Treatment Al Wheel Non-Heat Treatment Al Wheel
Al Si 7 Mg Sr Al Si 11 Mg Sr
Si 6.5 - 7.5 Si 10.5 - 11.5
Fe < 0.15 Fe < 0.15
Mg 0.25 - 0.30 Mg 0.10 - 0.30
Ti 0.10 - 0.15 Ti 0.10 - 0.15
Cu < 0.03 Cu < 0.03
Sr 0.01- 0.02 Sr 0.015 - 0.035

Mechanical Properties on Aluminium Wheel Casting

  Heat Treated Non-Heat Treated
Tensile Strength 250 N/mm2 150 N/mm2
Yield point 180 - 200 N/mm2 80 N/mm2
Elongation A5 5% 5%

Above data are for reference only.

 